1

1. Winding link: It can only be used when the diameter of the heating wire is less than 0.5mm. When the diameter of the heating wire is greater than 0.5mm, it is not easy to wind tightly, and the contact resistance is large.

2. The internal heating wire of the quartz tube is crimped with stainless steel skin.

3. Riveting.

U-shape-infrared-carbon-fiber-crystal-heating (2)

4. Spiral butt welding or milling groove cooling pressure. These two kinds of connection effect are better, but corresponding mechanical equipment is required.

When repairing the heating wire of iron-chromium-aluminum material, try to heat it to a dark fuchsia state as much as possible to prevent the heating wire from breaking.

14


Related Products

Category

Product Recommended

  • Silicone Heating Strips in Refrigeration Compressor Systems
  • Adjustable Electric Iron Kst Thermostat
  • Cut Off Fuse
  • High Density Cartridge Heater
  • Silicone Rubber Heater Mat With Adhesive
  • Oven Timer Switch For Cooking Appliance

Share